˻. Anti-Rust Method
           Metal corrosion is caused by various internal and external factors. Some common factors and corresponding countermeasures are listed
           below.

                   Factors aff ecting the corrosion of metal  Countermeasures to slow down rusting
                                                   Adopt materials with stronger anti-rust ability. For anti-rust ability
             1  Chemical composition and structure of metal itself
                                                   comparison of materials, refer to Table 1 on P.977.
                                                   Adopt surface treatments with stronger anti-rust ability. For anti-rust
             2  Surface treatment method of metal
                                                   ability comparison of surface treatments, refer to Table 2 on P.977.
             3  Metal surface fi nish               Select products with high processing accuracy

                                                   Avoid contact with media that tend to cause rusting of the material rust, such as hand sweat.
             4  Media composition in contact with metal surface
                                                   Regularly spray anti-rust oil. Refer to Table 3 on this page for the eff ect of spraying anti-rust oil.
               The higher the ambient temperature and humidity, the
             5                                     Maintain a low humidity and temperature environment.
               more easily the metal corrodes.

           Test Method:   Conduct the composite corrosion test according to GB/T 20854ˋ2007 cyclic test method
                                                     }
           Test Conditions:  ΍ Salt Water Spray Test (5%NaCl.35˫)  2hr
                       Ύ Dry (60˫ )               4hr    8hr is one cycle
                       Ώ Wet (95%RH. 35˫p2˫ )     2hr

           Comparison of Corrosion of SUJ2 Material (Without Surface Treatment) under Diff erent Maintenance
           Conditions (Reference)                                                             Table 3
                                                 Whether anti-rust oil is sprayed
           Placement Time
                                      Provided                            Not Provided



             Before Test






                8hr






               24hr











                                                                                                   978